Ni-, Co-, Fe-based

53-150 µm (standard) 
180-780 HV30

Ni based alloys provide good wear protection and corrosion resistance. Co based alloys retain most of the properties observed at room temperature even with increasing temperature. Iron based alloys are cost effective but heat and creep resistance can restrict their use.

Therefore application demands dictate correct material choise.

Quick Guide

Surfit™

Typical Hardness HV30

Typical Hardness HRC

Alloy Base

Article Nr.

1550 580 52 Ni 115955
1560 810 62 Ni 115956
2537 400  41 Co 117730
2541 430 44 Co 117731
316L 160   Fe 117729

News RSS for News

4th International Surface Engineering Expo 2014

4th International Surface Engineering Expo 2014 will take place 25th to 27th July in Shanghai, China. Meet us at stand number A018.

Metalloobrabotka 2014

Metalloobrabotka 2014 will take place 16th to 20th June in Moscow, Russia. Meet us at stand number 84c25.

Beijing Essen Welding & Cutting 2014

Beijing Essen Welding & Cutting 2014 will take place 10th to 13th June in Beijing, China. Meet us at stand number W1561.
All news items